Jump to content

Recommended Posts

Posted

What process do people use on pitted, surface rust and bare metal?!

 

I go for Kursust on the pitted areas, then upol etch and then highbuild.

 

Tempted to try mammerite anti-rust for a nice coverage and they do a rust beater?! And what about good old redoxide . . .

 

Opionions please thanks Charlie.

Posted

S6300122.jpg

A twist knot wire brush wheel on a grinder,It digs out paint and rust but leaves good metal(not me in pic).Or shot blast the rusty area with a spot blast gun which are cheap enough.Follow by a good zinc based primer :thumbsup:

Posted
Yer i do always cut out the rot, but some places arent rusty enought that they warrant cutting out and re - welding. On loads of places on old fords there surface rust :roll:

 

I know what you mean :lol:

 

There is some stuff called jenolite thats used by the MOD (ministry of defence) its meant to be really good but i havent tried mine out yet as I have no rust left now :lol:

Posted

I've always used Kurust then a good thick primer, usually the brush on stuff as the brush marks can be sanded out. Surface rust under the car is wire brushed, Kurust, then hammesh*te underseal or stonechip on top of that if it's the floor, fuel tank etc.

Posted

I have got the same prob with my mk2 escort the inside of the roof skin has got a layer of surface rust on it and i dont want to my grinder to it in fear of f**king the most expensive panel on the car !!! My dad says there used to be a liquid of some sort called POR 51 i think, he did some real tight spots on his 1071s cooper with it.

Posted
My dad says there used to be a liquid of some sort called POR 51 i think, he did some real tight spots on his 1071s cooper with it.

 

There is some rust prevention called por 15. Meant to be pretty good!

Posted

the best bet i thinks is to shot blast it being carefull not to damage the shape of the panel!!!! then if a hole appears cut it out and weld new in!!! and if in doubt give it a good treating with jenolite and scrub it in with a wire brush as it seems to penetrate better!!!! you can primer over jenolite within the hour which makes it quick and means that you captivate the fresh steel before it starts reacting again!!!

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
×
×
  • Create New...